Albroswift Posted September 27, 2021 Report Posted September 27, 2021 Any idea how hot an AR plastic hand guard can go? is 250 deg f too much heat?
Armed Eye Doc Posted September 28, 2021 Report Posted September 28, 2021 Calling @98Z5V. I know he has done plenty of Cerakote on all manor of material.
Albroswift Posted September 28, 2021 Author Report Posted September 28, 2021 It's from Armalite, not a knock off.
98Z5V Posted September 28, 2021 Report Posted September 28, 2021 I cure plastic at 170* for 3 hours, brother. Magpul handgrips , magazines and stocks, that sort of thing. This one that you have would fall right in there.
Albroswift Posted September 29, 2021 Author Report Posted September 29, 2021 Copy. I can do that. Thanks.
Albroswift Posted November 1, 2021 Author Report Posted November 1, 2021 On 9/28/2021 at 7:53 AM, 98Z5V said: I cure plastic at 170* for 3 hours Solid advice, went 3/ 18 minute flash coats at 170, stripped the stencils, and then a 2-1/2 hr cure at 175 Base coat Graphite Black, Then Snow White and Tactical Gray.
Recommended Posts
Create an account or sign in to comment
You need to be a member in order to leave a comment
Create an account
Sign up for a new account in our community. It's easy!
Register a new accountSign in
Already have an account? Sign in here.
Sign In Now